Aligning ball bearings are designed to automatically adjust the deflection of the shaft and housing or the misalignment of the shaft caused by different cores. It can bear radial load and bidirectional axial load. Suitable for use with light load, low impact load and high speed. Multi-purpose stamping iron and engineering plastics as cage. It is mainly used in precision instrument, low noise motor, automobile, motorcycle and general machinery.
Main material | ||
Name of engineering plastics | Abbreviation code | Temperature range(ºC) |
Glass fiber reinforced polyamide 66 | PA66-GF30 | -40-120 |
PA66-GF25 | -40-120 | |
PA66-GF15 | -40-110 | |
PA66-GF10 | -40-110 | |
Polyamide 66 | PA66 | -40-90 |
Glass fiber reinforced polyamide 46 | PA46-GF30 | -40-160 |
PA46-GF25 | -40-150 | |
PA46-GF15 | -40-130 | |
Polyamide 46 | PA46 | -40-110 |
Others | PI | >200 |
PEEK | ||
PAEK | ||
PC | <100 | |
PP | ||
PE |
Main material property | ||||||||||
Serial | Varieties | PA66-GF25 | PA66-GF30 | PA66-GF15 | PA66-GF10 | PA66 | PA46-GF30 | PA46-GF25 | PA46-GF15 | PA46 |
1 | Appearance | Fine grain, no obvious color difference, no coke particles. | ||||||||
2 | melting point(ºC) | >255 | >295 | |||||||
3 | density(g/cm3) | 1.29~1.35 | 1.33~1.39 | 1.20~1.26 | 1.17~1.23 | 1.11~1.17 | 1.39~1.43 | 1.33~1.37 | 1.27~1.31 | 1.16~1.2 |
4 | Water absorbability(%) | <=1 | <=1 | <=1 | <=1.2 | <=1.5 | <=2.6 | <=2.8 | <=3.1 | <=3.7 |
5 | Glass fiber content(%) | 23~27 | 28~32 | 13~17 | 8~12 | - | 28~32 | 23~27 | 13~17 | - |
6 | tensile strength Mpa | >150 | >160 | >110 | >80 | >70 | >180 | >170 | >117 | >87 |
7 | impact strength (KJ/m2) | >42 | >50 | >35 | >28 | >60 | >80 | >70 | >50 | - |
8 | ball indentation hardness(MPa) | >200 | >210 | >170 | >160 | >130 | >220 | >205 | >190 | >170 |
9 | Bending spring modulus (Gpa) | >6 | >7 | >5 | >4 | >2.5 | >9 | >7.5 | >6 | >3 |
10 | Hot deformation temperature(1.8MPa)ºC | >240 | >240 | >240 | >220 | >70 | >290 | >280 | >275 | >190 |
ps:Glass fiber is surface treated alkali free short glass fiber. |
Shipping Details
Samples by express like DHL. UPS .FedEx.TNT etc.
Goods by air cargo or by Sea.
Sample lead time: 1-2 days for stocked model. 5~10 days for customize samples.
Mass production time: 20-35 days for order.
Aligning ball bearings are designed to automatically adjust the deflection of the shaft and housing or the misalignment of the shaft caused by different cores. It can bear radial load and bidirectional axial load. Suitable for use with light load, low impact load and high speed. Multi-purpose stamping iron and engineering plastics as cage. It is mainly used in precision instrument, low noise motor, automobile, motorcycle and general machinery.
Main material | ||
Name of engineering plastics | Abbreviation code | Temperature range(ºC) |
Glass fiber reinforced polyamide 66 | PA66-GF30 | -40-120 |
PA66-GF25 | -40-120 | |
PA66-GF15 | -40-110 | |
PA66-GF10 | -40-110 | |
Polyamide 66 | PA66 | -40-90 |
Glass fiber reinforced polyamide 46 | PA46-GF30 | -40-160 |
PA46-GF25 | -40-150 | |
PA46-GF15 | -40-130 | |
Polyamide 46 | PA46 | -40-110 |
Others | PI | >200 |
PEEK | ||
PAEK | ||
PC | <100 | |
PP | ||
PE |
Main material property | ||||||||||
Serial | Varieties | PA66-GF25 | PA66-GF30 | PA66-GF15 | PA66-GF10 | PA66 | PA46-GF30 | PA46-GF25 | PA46-GF15 | PA46 |
1 | Appearance | Fine grain, no obvious color difference, no coke particles. | ||||||||
2 | melting point(ºC) | >255 | >295 | |||||||
3 | density(g/cm3) | 1.29~1.35 | 1.33~1.39 | 1.20~1.26 | 1.17~1.23 | 1.11~1.17 | 1.39~1.43 | 1.33~1.37 | 1.27~1.31 | 1.16~1.2 |
4 | Water absorbability(%) | <=1 | <=1 | <=1 | <=1.2 | <=1.5 | <=2.6 | <=2.8 | <=3.1 | <=3.7 |
5 | Glass fiber content(%) | 23~27 | 28~32 | 13~17 | 8~12 | - | 28~32 | 23~27 | 13~17 | - |
6 | tensile strength Mpa | >150 | >160 | >110 | >80 | >70 | >180 | >170 | >117 | >87 |
7 | impact strength (KJ/m2) | >42 | >50 | >35 | >28 | >60 | >80 | >70 | >50 | - |
8 | ball indentation hardness(MPa) | >200 | >210 | >170 | >160 | >130 | >220 | >205 | >190 | >170 |
9 | Bending spring modulus (Gpa) | >6 | >7 | >5 | >4 | >2.5 | >9 | >7.5 | >6 | >3 |
10 | Hot deformation temperature(1.8MPa)ºC | >240 | >240 | >240 | >220 | >70 | >290 | >280 | >275 | >190 |
ps:Glass fiber is surface treated alkali free short glass fiber. |
Shipping Details
Samples by express like DHL. UPS .FedEx.TNT etc.
Goods by air cargo or by Sea.
Sample lead time: 1-2 days for stocked model. 5~10 days for customize samples.
Mass production time: 20-35 days for order.
Home | Products | Company Profile | Contact Us | Download | Privacy Policy